The industrial-scale simulation unit for the electrochemical electrolysis of acrylonitrile to adiponitrile employs a membrane-free electrolytic cell with an electrode area of 1.5 cm², electrode spacing of 2 mm, and an electrolyte flow rate of 2 m/s within the cell. The unit features a compact design with minimal space occupation, achieving a selectivity of up to 85% in electrolytic experiments and a current efficiency exceeding 86%.
The industrial-scale simulation unit for the electrochemical electrolysis of acrylonitrile to adiponitrile employs a membrane-free electrolytic cell with an electrode area of 1.5 cm², electrode spacing of 2 mm, and an electrolyte flow rate of 2 m/s within the cell. The unit features a compact design with minimal space occupation, achieving a selectivity of up to 85% in electrolytic experiments and a current efficiency exceeding 86%.